BODYCOTE THERMAL PROCESSING -
NADCAP Approved
90049129
Independent Processor
3370 BENEDICT WAY
HUNTINGTON PARK , CA 90255-4517 United States
Phone: 323-583-1231
Fax:
90049129
Independent Processor
3370 BENEDICT WAY
HUNTINGTON PARK , CA 90255-4517 United States
Phone: 323-583-1231
Fax:
Selected sector: AS
Specification
ProcessDescription
Category
Heat Treatment of Carbon and Low-Alloy Steel Parts Min Ten. Str.< 220ksi
Heat Treat
Limits:
None
Stress relief of steel parts
Heat Treat
Limits:
None
Heat Treatment of Carbon and Low-Alloy Steel Parts Min Ten. Str.> 220ksi
Heat Treat
Limits:
None
Heat Treatment Precipitation-Hardening CRES and Maraging Steel Parts
Heat Treat
Limits:
None
Heat Treatment Martensitic Corrosion Resistant Steel Parts
Heat Treat
Limits:
None
Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts
Heat Treat
Limits:
None
Carburizing and Heat Treatment of Carburizing Grade Steel Parts
Heat Treat
Limits:
None
Heat Treatment of Steel Raw Materials
Heat Treat
Limits:
None
Heat Treatment Nickel Alloy and Cobalt Alloy Parts
Heat Treat
Limits:
None
Cleaning Prior to Plating Low Alloy Steel
Chemical Processing
Limits:
Brulin 815GD is approved for use per RCI 120723
Removal of Copper Barrier Coatings - Low Alloy Steel
Chemical Processing
Limits:
None
Abrasive Cleaning
Chemical Processing
Limits:
None
Cleaning Prior to Heat Treat Carbon & Low Alloy Steels
Chemical Processing
Limits:
Limited to solvent clean only
Heat Treatment of Low Alloy Steel
Heat Treat
Limits:
Limited to alloys less than 220 KSI. Do not process any material at 220 KSI and up
Heat Treatment of Wrought Precipitation Hardenable Stainless Steel.
See Supplier for Custom 465
Heat Treat
Limits:
Not Approved for Custom 465
Heat Treatment of Steel Parts, <220 Ksi
Heat Treat
Limits:
None
Heat Treatment of Precipitation Hardening Corrosion Resistant Steels
Heat Treat
Limits:
Excludes 17-7 PH in the following conditions TH1050, TH1080, and TH1100
Heat Treatment of Carbon and Alloy Steels up to 200,000 psi
Heat Treat
Limits:
None
Heat Treatment of Low Alloy Steels From 200,000 to 260,000 psi
Heat Treat
Limits:
None