Specification ProcessDescription Category SpecLimits
AMS 2759/ 1 Heat Treatment of Carbon and Low-Alloy Steel Parts Min Ten. Str.< 220ksi Heat Treat Limits: None
AMS 2759/11 Stress relief of steel parts Heat Treat Limits: None
AMS 2759/2 Heat Treatment of Carbon and Low-Alloy Steel Parts Min Ten. Str.> 220ksi Heat Treat Limits: None
AMS 2759/3 Heat Treatment Precipitation-Hardening CRES and Maraging Steel Parts Heat Treat Limits: None
AMS 2759/5 Heat Treatment Martensitic Corrosion Resistant Steel Parts Heat Treat Limits: None
AMS 2759/6 Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts Heat Treat Limits: None
AMS 2759/7 Carburizing and Heat Treatment of Carburizing Grade Steel Parts Heat Treat Limits: None
AMS 2761 Heat Treatment of Steel Raw Materials Heat Treat Limits: None
AMS 2774 Heat Treatment Nickel Alloy and Cobalt Alloy Parts Heat Treat Limits: None
C-18 Cleaning Prior to Plating Low Alloy Steel Chemical Processing Limits: Brulin 815GD is approved for use per RCI 120723
C-20 Removal of Copper Barrier Coatings - Low Alloy Steel Chemical Processing Limits: None
C-47 Abrasive Cleaning Chemical Processing Limits: None
C-52 Cleaning Prior to Heat Treat Carbon & Low Alloy Steels Chemical Processing Limits: Limited to solvent clean only
GSS 5100 Heat Treatment of Low Alloy Steel Heat Treat Limits: Limited to alloys less than 220 KSI.
GSS 5102 Heat Treatment of Wrought Precipitation Hardenable Stainless Steel. See Supplier for Custom 465 Heat Treat Limits: Not Approved for Custom 465
H-105 Heat Treatment of Steel Parts, <220 Ksi Heat Treat Limits: None
HT-19 Heat Treatment of Precipitation Hardening Corrosion Resistant Steels Heat Treat Limits: Excludes 17-7 PH in the following conditions TH1050, TH1080, and TH1100
HT-21 Heat Treatment of Carbon and Alloy Steels up to 200,000 psi Heat Treat Limits: None
HT-22 Heat Treatment of Low Alloy Steels From 200,000 to 260,000 psi Heat Treat Limits: None