Specification
|
ProcessDescription
|
Category
|
SpecLimits
|
AMS 2759
|
General Requirements for Heat Treatment of Steel Parts
|
Heat Treat
|
Limits:
None
|
AMS 2759/3
|
Heat Treatment Precipitation-Hardening CRES and Maraging Steel Parts
|
Heat Treat
|
Limits:
None
|
AMS 2761
|
Heat Treatment of Steel Raw Materials
|
Heat Treat
|
Limits:
None
|
AMS 2772
|
Heat Treatment of Aluminum Alloy Raw Materials
|
Heat Treat
|
Limits:
None
|
AMS-H-81200
|
Heat Treatment of Titanium and Titanium Alloys
|
Heat Treat
|
Limits:
None
|
H-102
|
Heat Treatment of Titanium Parts
|
Heat Treat
|
Limits:
Limited to stress relief only. Deviation approved per RC/I BR406072, BR406314 and ESP H102 |
H-110
|
Heat Treatment of Precipitation Hardening CRES Parts
|
Heat Treat
|
Limits:
Limited to straightening & stress relief per R-303 only |
HT-21
|
Heat Treatment of Carbon and Alloy Steels up to 200,000 psi
|
Heat Treat
|
Limits:
Limited to approved RCI TS-11-189-04 & TS-13-249-01 |
LMA-PC009
|
Hardness and Conductivity Testing
|
Miscellaneous
|
Limits:
Approval based on QCS-001 and subject to the limitations on QCS-001 |
R-301
|
Straightening Aluminum and 17-4 PH CRES Castings
|
Miscellaneous
|
Limits:
Straightening 17-4PH CRES Castings only |
R-303
|
Straightening Wrought CRES Alloys
|
Miscellaneous
|
Limits:
None
|
R-304
|
Straightening Titanium Forgings and Extrusions
|
Miscellaneous
|
Limits:
Deviation approved per RC/I BR406072, BR406314 and R-304 |