Specification
|
ProcessDescription
|
Category
|
SpecLimits
|
AMS 2759
|
General Requirements for Heat Treatment of Steel Parts
|
Heat Treat
|
Limits:
Vacuum or retort HT only. Parts are to be cleaned by customer |
AMS 2759/ 1
|
Heat Treatment of Carbon and Low-Alloy Steel Parts Min Ten. Str.< 220ksi
|
Heat Treat
|
Limits:
Vacuum or Retort HT only. Parts to be cleaned by customer. |
AMS 2759/2
|
Heat Treatment of Carbon and Low-Alloy Steel Parts Min Ten. Str.> 220ksi
|
Heat Treat
|
Limits:
Vacuum or Retort HT only. Parts to be cleaned by customer. |
AMS 2759/3
|
Heat Treatment Precipitation-Hardening CRES and Maraging Steel Parts
|
Heat Treat
|
Limits:
Vacuum or Retort HT only. Parts to be cleaned by customer. |
AMS 2759/4
|
Heat Treatment Austenitic Corrosion-Resistant Steel Parts
|
Heat Treat
|
Limits:
Vacuum or Retort HT only. Parts to be cleaned by customer. |
AMS 2759/5
|
Heat Treatment Martensitic Corrosion Resistant Steel Parts
|
Heat Treat
|
Limits:
Vacuum or Retort HT only. Parts to be cleaned by customer. |
AMS 2774
|
Heat Treatment Nickel Alloy and Cobalt Alloy Parts
|
Heat Treat
|
Limits:
Vacuum or Retort HT only. Parts to be cleaned by customer. |
AMS 2801
|
Heat Treatment of Titanium Alloy Parts
|
Heat Treat
|
Limits:
Vacuum or Retort HT only. Parts must be cleaned by customer. |
AMS-H-6875
|
Heat Treatment of Steel Raw Materials
|
Heat Treat
|
Limits:
Vacuum or Retort HT
only. Parts must be
cleaned by customer. |
AMS-H-81200
|
Heat Treatment of Titanium and Titanium Alloys
|
Heat Treat
|
Limits:
Vacuum or Retort HT only. Parts must be cleaned by customer. |
GSS 5102
|
Heat Treatment of Wrought Precipitation Hardenable Stainless Steel.
See Supplier for Custom 465
|
Heat Treat
|
Limits:
Limited to stress relief only. Excludes pre-cleaning, post cleaning, and descaling. |
GSS 5150
|
Heat Treatment of Titanium and Titanium Alloys
|
Heat Treat
|
Limits:
Parts must be cleaned by customer prior to Heat Treat processing. |