| Specification | ProcessDescription | Category | SpecLimits |
| ACS-PRS-1053 | Process Specification for Etching Prior to Penetrant Inspection | Chemical Processing | Limits: Limited to aluminum and stainless steel only |
| ACS-PRS-7005 | Penetrant Inspection | Non-Destructive Testing | Limits: Not approved for Appendix A & B |
| AMS 2404 | Plating, Electroless Nickel | Chemical Processing | Limits: None |
| AMS 2460 | Plating, Chromium | Chemical Processing | Limits: Type II only |
| AMS 2700 | Passivation Treatments for Corrosion-Resistant Steel | Chemical Processing | Limits: Method 1, Type 2, 6 & 8 only |
| AMS-QQ-N-290 | Nickel Plating (Electrodeposited) | Chemical Processing | Limits: None |
| ASTM A380 | Cleaning, Descaling, and Passivation of Stainless Steel | Chemical Processing | Limits: None |
| ASTM B117 | Standard Practice for Operating Salt Spray (Fog) Apparatus | Non-Destructive Testing | Limits: In-house testing only |
| ASTM E1417 | Standard Practice for Liquid Penetrant Testing | Non-Destructive Testing | Limits: None |
| ASTM E1444 | Standard Practice for Magnetic Particle Testing | Non-Destructive Testing | Limits: None |
| MIL-DTL-18264 | Finishes Organic, Weapons System, Application and Control of | Chemical Processing | Limits: None |
| MIL-DTL-5541 | Chemical Conversion Coatings for Aluminum and Aluminum Alloy | Chemical Processing | Limits: Limited to Type 1 only |
| MIL-F-18264 | Finishes Organic, Weapons System, Application and Control of | Chemical Processing | Limits: None |
| MIL-PRF-46010 | Dry Film Lube Superseded by AS5272 for Ty I & II only | Chemical Processing | Limits: None |
| MIL-PRF-8625 | Anodic Coatings For Aluminum and Aluminum Alloys | Chemical Processing | Limits: Dichromate seal is required when MIL-PRF-8625 Type II anodize is called out on engineering drawings. |